窒化・酸化・浸炭競合環境における ステンレス鋼製加熱管の減肉機構解明
著者:
山本 康平,Kohei YAMAMOTO,阿部 博志,Hiroshi ABE,渡邉 豊,Yutaka WATANABE,有岡 真平,Shinpei ARIOKA,小野 雅史,Masashi ONO
発刊日:
公開日:
キーワードタグ:
It was reported that nitride layer formed on SUS310S heating tubes in the reactor of melamine production plant showed severe spalling susceptibility. After replacement to SUS304heating tubes, spalling and thinning was suppressed. According to previous studies, a crystal structure of the nitrided layers of SUS310S and SUS304 heating tubes mainly consist of γ’ and α’, respectively. The reason why the SUS304 heating tube showed low spalling susceptibility was considered to be a smaller expansion rate of α...
英字タイトル:
Wastage mechanism of heating tubes made of austenitic stainless steels in a complex environment of nitriding, oxidizing, and carburizing